18HGT
Case hardening steel
![stal do naweglania](https://multistal.pl/wp-content/uploads/2021/09/stal-do-naweglania.webp)
Dimensions:
![](https://multistal.pl/wp-content/themes/multistal/img/content/pictogram1.png)
from Φ 20 mm to Φ 500 mm in diameter
Chemical composition:
Element | C | Si | Mn | P | S | Cr | W | V | Ni | Ti | Cu |
---|---|---|---|---|---|---|---|---|---|---|---|
min | 0.17 | 0.17 | 0.8 | max | max | 1.1 | max | max | max | 0.05 | max |
max | 0.23 | 0.37 | 1.1 | 0.035 | 0.035 | 1.3 | 0.2 | 0.05 | 0.3 | 0,12 | 0.3 |
Equivalents:
Wr.Nr. | PN | EN | GOST | AISI |
---|---|---|---|---|
– | 18HGT | – | 18ХГТ | – |
Delivery condition:
Round bars:
- +A – annealed
- +U – untreated
Description:
High strength steel for machine parts. Can be machined, suitable for cutting. Welding is possible after preheating, before carburizing.
Applications:
Steel for loaded parts requiring high core strength: gears, shafts.
Dimensions:
![](https://multistal.pl/wp-content/themes/multistal/img/content/pictogram1.png)
from Φ 20 mm to Φ 500 mm in diameter
Chemical composition:
Element | C | Si | Mn | P | S | Cr | W | V | Ni | Ti | Cu |
---|---|---|---|---|---|---|---|---|---|---|---|
min | 0.17 | 0.17 | 0.8 | max | max | 1.1 | max | max | max | 0.05 | max |
max | 0.23 | 0.37 | 1.1 | 0.035 | 0.035 | 1.3 | 0.2 | 0.05 | 0.3 | 0,12 | 0.3 |
Equivalents:
Wr.Nr. | PN | EN | GOST | AISI |
---|---|---|---|---|
– | 18HGT | – | 18ХГТ | – |