1.4762; X10CrAlSi24

Heat resistant ferritic steel

Dimensions:
Chemical composition:
Element C Si Mn P S Cr Al
min max. 0.70 max. max max 23.00 1.20
max 0.12 1.40 1.0 0.04 0.015 26.00 1.70
Equivalents:
Wr.Nr. PN EN GOST AISI
1.4762 X10CrAl25 15Х28 446
Delivery condition:

Sheet metal & plates :

  • +A – annealed
Description:

1.4762; AISI 446 is a rustproof, heat-resistant ferritic chromium steel with an aluminum additive. Special properties Resistant to scaling up to 1150°C. Resistant to oxidizing sulfurous gases.

Applications:

Conductor stripes for steam boiler super heater etc.

Chemical composition:
Element C Si Mn P S Cr Al
min max. 0.70 max. max max 23.00 1.20
max 0.12 1.40 1.0 0.04 0.015 26.00 1.70
Equivalents:
Wr.Nr. PN EN GOST AISI
1.4762 X10CrAl25 15Х28 446